Question£º |
Orange surface |
reason£º |
In 1, the spraying pressure is too large, spraying uneven thickness
In 2, the powder agglomeration, the atomization degree difference |
resolvent |
1, proficient in spraying technology
2, do not use powder agglomeration, adjustment of gun powder atomization |
|
|
Question£º |
Chromatic aberration |
reason£º |
In 1, the baking time is too long and too short, the baking temperature is too high or too low
2, oven temperature anomaly |
resolvent |
1, to provide reference for powder curing condition adjustment
2, check the oven heating element condition |
|
|
Question£º |
Surface gloss |
reason£º |
In 1, adding a new powder powder recovery problems
2, different manufacturers or different types of powder mixing |
resolvent |
In 1, a moratorium on the use of problem of powder recovery
2, avoid mixing different powder |
|
|
|